High Strength 7050 Aluminum Sheet Plate Stress Corrosion Cracking Resistance

Ask Latest Price
Brand Name :HUANYU
Model Number :HYAP7050
Place of Origin :CHINA
MOQ :1 metric ton
Price :Negotiable
Payment Terms :T/T
Supply Ability :220 metric tons per month
Delivery Time :40 dyas
Packaging Details :Plywood Case
Applications :fuselage frames, bulkheads and wing skins
Characteristics :high mechanical properties and high fracture toughness
Performance subzero temperatures :high strength at subzero temperatures.
Corrosion Resistance :good exfoliation corrosion resistance
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

High Strength, Stress Corrosion Cracking Resistance 7050 Aluminum Sheet Plate

Aluminium alloy 7050
is an aerospace grade of aluminium combining high strength, stress corrosion cracking resistance and toughness.
It is particularly suited for heavy plate applications (3" to 6" thick) due to it's lower quench sensitivity and retention of strength in thicker sections.
Aluminium 7050 therefore is the premium choice aerospace aluminium for applications such as fuselage frames, bulkheads and wing skins.

7050 Aluminium Sheet Plate Chemical Composition

Chemical Composition Limits Aluminium Alloy 7050 Others
Weight % Al Zr Si Fe Cu Mn Mg Cr Zn Ti Each Total
Minimum 87.3 0.08 - - 2.0 - 1.90 - 5.7 - - -
Maximum 90.3 0.15 0.12 0.15 2.6 0.10 2.60 0.04 6.7 0.06 0.05 0.15

High Strength 7050 Aluminum Sheet Plate Stress Corrosion Cracking ResistanceHigh Strength 7050 Aluminum Sheet Plate Stress Corrosion Cracking ResistanceHigh Strength 7050 Aluminum Sheet Plate Stress Corrosion Cracking ResistanceHigh Strength 7050 Aluminum Sheet Plate Stress Corrosion Cracking Resistance